Zinc telluride single crystal
- Crystal structure : cubic, a = 6.1034Å
- Growth direction : <111>
- Orientation : (100) (110) (111) +/- 0.5°
- Growth method : Seeded Vapor-Phase Free Growth Technology
- Specific resistivity : 100 Ohm-cm
- Hall mobility : 130 (h) cm2/V-sec.
- EPD : < 5 X 105 / cm2
- Twin free
| Orientation |
Size |
Polish |
Price |
| ZnTe100) |
10 X 10 X 1mm3 |
both sides polished |
Quote |
| ZnTe(110) |
10 X 10 X 1mm3 |
both sides polished |
Quote |
| ZnTe(111) |
10 X 10 X 1mm3 |
both sides polished |
Quote |